Comparison of mechanical properties of different particle sizes of recycled polycarbonate at higher temperature
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28140%2F14%3A43872715" target="_blank" >RIV/70883521:28140/14:43872715 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/70883521:28110/14:43872715
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Comparison of mechanical properties of different particle sizes of recycled polycarbonate at higher temperature
Popis výsledku v původním jazyce
This research paper deals with behavior of particles of a recycled material at a higher temperature depending on the particle size. Behavior is tested by mechanical properties. During grinding particles are formed which have a different size, shape and surface, from larger pieces to dust particles. During processing these particles melt at different rates depending on their size. For example they can cause material degradation or lack of melt homogeneity. Several recycled mixtures were prepared that haddiffered particle size after crushing. The recycled material is always the same as is the original material. The studied material was high-heat polycarbonate. Testing was performed using a tensile test, Charpy impact test and hardness test. Specimens were prepared by the mostly used technology for production products, which is injection molding. Each mixture is one by one loaded by high temperature 100°C and consequently tested. This temperature was chosen because we encounter products
Název v anglickém jazyce
Comparison of mechanical properties of different particle sizes of recycled polycarbonate at higher temperature
Popis výsledku anglicky
This research paper deals with behavior of particles of a recycled material at a higher temperature depending on the particle size. Behavior is tested by mechanical properties. During grinding particles are formed which have a different size, shape and surface, from larger pieces to dust particles. During processing these particles melt at different rates depending on their size. For example they can cause material degradation or lack of melt homogeneity. Several recycled mixtures were prepared that haddiffered particle size after crushing. The recycled material is always the same as is the original material. The studied material was high-heat polycarbonate. Testing was performed using a tensile test, Charpy impact test and hardness test. Specimens were prepared by the mostly used technology for production products, which is injection molding. Each mixture is one by one loaded by high temperature 100°C and consequently tested. This temperature was chosen because we encounter products
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JP - Průmyslové procesy a zpracování
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED2.1.00%2F03.0089" target="_blank" >ED2.1.00/03.0089: Centrum bezpečnostních, informačních a pokročilých technologií (CEBIA-Tech)</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
International Journal of Mechanics
ISSN
1998-4448
e-ISSN
—
Svazek periodika
8
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
8
Strana od-do
268-275