Deposition of Non-Fouling PEO-Like Coatings Using a Low Temperature Atmospheric Pressure Plasma Jet
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F16%3A10329342" target="_blank" >RIV/00216208:11320/16:10329342 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1002/ppap.201500034" target="_blank" >http://dx.doi.org/10.1002/ppap.201500034</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1002/ppap.201500034" target="_blank" >10.1002/ppap.201500034</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Deposition of Non-Fouling PEO-Like Coatings Using a Low Temperature Atmospheric Pressure Plasma Jet
Popis výsledku v původním jazyce
Plasma polymerised PEO-like films were deposited from tetraethylene glycol dimethyl ether (TEGDME) and diethylene glycol vinyl ether (DEGVE) using an atmospheric plasma jet. Films formed from TEGDME with COC retention >50% showed anti-fouling properties, while DEGVE films with COC >60% did not. TEGDME films deposited at higher monomer flow rates had a lower density and more amorphous phases in the polymer network. Consequently, these films more readily facilitate penetration and binding of water to their surface in comparison to the denser DEGVE films. The difference in fouling properties identified through this comparative study has shown that % COC retention may not alone be an indication of non-fouling behaviour. Other factors such as polymer network structure may also play a crucial role in the prevention of surface fouling.
Název v anglickém jazyce
Deposition of Non-Fouling PEO-Like Coatings Using a Low Temperature Atmospheric Pressure Plasma Jet
Popis výsledku anglicky
Plasma polymerised PEO-like films were deposited from tetraethylene glycol dimethyl ether (TEGDME) and diethylene glycol vinyl ether (DEGVE) using an atmospheric plasma jet. Films formed from TEGDME with COC retention >50% showed anti-fouling properties, while DEGVE films with COC >60% did not. TEGDME films deposited at higher monomer flow rates had a lower density and more amorphous phases in the polymer network. Consequently, these films more readily facilitate penetration and binding of water to their surface in comparison to the denser DEGVE films. The difference in fouling properties identified through this comparative study has shown that % COC retention may not alone be an indication of non-fouling behaviour. Other factors such as polymer network structure may also play a crucial role in the prevention of surface fouling.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/LD12066" target="_blank" >LD12066: Zvýšení biokompatibility materiálů plazmovými technikami za atmosferického tlaku pro biolékařské aplikace</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Plasma Processes and Polymers
ISSN
1612-8850
e-ISSN
—
Svazek periodika
13
Číslo periodika v rámci svazku
2
Stát vydavatele periodika
DE - Spolková republika Německo
Počet stran výsledku
12
Strana od-do
241-252
Kód UT WoS článku
000370020100005
EID výsledku v databázi Scopus
2-s2.0-84959094092