In situ electrochemical AFM monitoring of the potential-dependent deterioration of platinum catalyst during potentiodynamic cycling
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216208%3A11320%2F18%3A10386158" target="_blank" >RIV/00216208:11320/18:10386158 - isvavai.cz</a>
Výsledek na webu
<a href="https://doi.org/10.1016/j.ultramic.2018.01.015" target="_blank" >https://doi.org/10.1016/j.ultramic.2018.01.015</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.ultramic.2018.01.015" target="_blank" >10.1016/j.ultramic.2018.01.015</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
In situ electrochemical AFM monitoring of the potential-dependent deterioration of platinum catalyst during potentiodynamic cycling
Popis výsledku v původním jazyce
A platinum catalyst undergoes complex deterioration process during its operation as a cathode in a proton exchange membrane fuel cell. By using in situ electrochemical atomic force microscopy (EC-AFM) with super-sharp probes, we quantitatively describe the roughening of platinum thin films during electrochemical cycling to different upper potentials, which simulate critical operation regimes of the proton exchange membrane fuel cell. The comprehensive quantitative analysis of morphology changes obtained using common roughness descriptors such as the root mean square roughness, the correlation length and the roughness exponent is correlated with cyclic voltammetry performed simultaneously.
Název v anglickém jazyce
In situ electrochemical AFM monitoring of the potential-dependent deterioration of platinum catalyst during potentiodynamic cycling
Popis výsledku anglicky
A platinum catalyst undergoes complex deterioration process during its operation as a cathode in a proton exchange membrane fuel cell. By using in situ electrochemical atomic force microscopy (EC-AFM) with super-sharp probes, we quantitatively describe the roughening of platinum thin films during electrochemical cycling to different upper potentials, which simulate critical operation regimes of the proton exchange membrane fuel cell. The comprehensive quantitative analysis of morphology changes obtained using common roughness descriptors such as the root mean square roughness, the correlation length and the roughness exponent is correlated with cyclic voltammetry performed simultaneously.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10305 - Fluids and plasma physics (including surface physics)
Návaznosti výsledku
Projekt
<a href="/cs/project/EF16_013%2F0001788" target="_blank" >EF16_013/0001788: Laboratoř fyziky povrchů - Optická dráha pro výzkum materiálů</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach<br>I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2018
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Ultramicroscopy
ISSN
0304-3991
e-ISSN
—
Svazek periodika
187
Číslo periodika v rámci svazku
Apr
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
7
Strana od-do
64-70
Kód UT WoS článku
000428131200009
EID výsledku v databázi Scopus
2-s2.0-85041384506