The change chemical composition and thermophysical properties of concast steel slab and their relation to breakout
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F10%3APU88458" target="_blank" >RIV/00216305:26210/10:PU88458 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
The change chemical composition and thermophysical properties of concast steel slab and their relation to breakout
Popis výsledku v původním jazyce
In the secondary-cooling zone, where the slab is beginning to straighten out the breakout of the steel can occur in points of increased local chemical and temperature heterogeneity of the steel, from increased tension as a result of the bending of the slab and also from a high local concentration of non-metal, slag inclusions. Especially dangerous are the changes in the chemical composition of the steel during the actual concasting. In the case of two melts one immediately after the other, this could lead to immediate interruption in the concasting and a breakout. The material, physical, chemical and technological parameters, which both melts differed in were determined. If the dimensionless analysis is applied for assessing and reducing the number ofthese parameters, then it is possible to express the level of risk of breakout as a function of five dimensionless criteria.
Název v anglickém jazyce
The change chemical composition and thermophysical properties of concast steel slab and their relation to breakout
Popis výsledku anglicky
In the secondary-cooling zone, where the slab is beginning to straighten out the breakout of the steel can occur in points of increased local chemical and temperature heterogeneity of the steel, from increased tension as a result of the bending of the slab and also from a high local concentration of non-metal, slag inclusions. Especially dangerous are the changes in the chemical composition of the steel during the actual concasting. In the case of two melts one immediately after the other, this could lead to immediate interruption in the concasting and a breakout. The material, physical, chemical and technological parameters, which both melts differed in were determined. If the dimensionless analysis is applied for assessing and reducing the number ofthese parameters, then it is possible to express the level of risk of breakout as a function of five dimensionless criteria.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2010
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Acta metalurgica slovaca
ISSN
1338-1660
e-ISSN
—
Svazek periodika
1
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
SK - Slovenská republika
Počet stran výsledku
6
Strana od-do
—
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—