K-calibration of Special Specimens for Mode II, III and II+III Crack Growth
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F13%3APU105536" target="_blank" >RIV/00216305:26210/13:PU105536 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.engfracmech.2013.08.013" target="_blank" >http://dx.doi.org/10.1016/j.engfracmech.2013.08.013</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.engfracmech.2013.08.013" target="_blank" >10.1016/j.engfracmech.2013.08.013</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
K-calibration of Special Specimens for Mode II, III and II+III Crack Growth
Popis výsledku v původním jazyce
An original testing setup has been designed for generating pure remote mode II, III and mixed mode II + III crack propagation in a single cylindrical specimen with circumferential crack. This specimen is currently used for investigations of a shear modefatigue crack propagation. The aim of this work was to perform the K-calibration of above mentioned specimens that will be used for a description of stability and growth of shear-mode fatigue cracks in the near-threshold region. Two-step submodelling based on the ANSYS code was performed in order to obtain sufficiently precise values of the stress intensity factors KII, KIII and KII,III along the crack front of small and large samples. The shape functions FII, FIII and FII,III were determined using theJ-integral concept. The calculated values of the KIII factors could be, unlike those of KII factors, nearly compared with the solution based on an asymptotic approximation available in the literature. Calculations revealed that, for small
Název v anglickém jazyce
K-calibration of Special Specimens for Mode II, III and II+III Crack Growth
Popis výsledku anglicky
An original testing setup has been designed for generating pure remote mode II, III and mixed mode II + III crack propagation in a single cylindrical specimen with circumferential crack. This specimen is currently used for investigations of a shear modefatigue crack propagation. The aim of this work was to perform the K-calibration of above mentioned specimens that will be used for a description of stability and growth of shear-mode fatigue cracks in the near-threshold region. Two-step submodelling based on the ANSYS code was performed in order to obtain sufficiently precise values of the stress intensity factors KII, KIII and KII,III along the crack front of small and large samples. The shape functions FII, FIII and FII,III were determined using theJ-integral concept. The calculated values of the KIII factors could be, unlike those of KII factors, nearly compared with the solution based on an asymptotic approximation available in the literature. Calculations revealed that, for small
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JL - Únava materiálu a lomová mechanika
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Engineering Fracture Mechanics
ISSN
0013-7944
e-ISSN
—
Svazek periodika
110
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
8
Strana od-do
430-437