Fracture toughness transition of ferritic-pearlitic steel at static and dynamic loading evaluated by master curve concept
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F00216305%3A26210%2F18%3APU128477" target="_blank" >RIV/00216305:26210/18:PU128477 - isvavai.cz</a>
Výsledek na webu
<a href="http://ojs.mateng.sk/index.php/Mateng/article/view/229/431" target="_blank" >http://ojs.mateng.sk/index.php/Mateng/article/view/229/431</a>
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Fracture toughness transition of ferritic-pearlitic steel at static and dynamic loading evaluated by master curve concept
Popis výsledku v původním jazyce
The paper focuses on assessing the usability of fatigue pre-cracked Charpy type specimens when evaluating the resistance of steel with ferritic-pearlitic structure to the initiation of unstable fractures. The suitability of using the specimens is evaluated on the basis of comparing experimentally established values of fracture toughness on pre-cracked Charpy type specimens and the values of this characteristics determined using Compact Tension (CT) specimens. For the evaluation and comparison of the fracture toughness temperature dependences determined on individual specimen types the master curve concept quantifying fracture toughness transition was applied. In the case of the steel employed, very good agreement was found to exist between the characteristics determined on individual types of specimen. It was shown that fracture toughness determined on pre-cracked Charpy type specimens can be regarded as a representative measure of resistance of the material employed to the brittle fracture occurrence.
Název v anglickém jazyce
Fracture toughness transition of ferritic-pearlitic steel at static and dynamic loading evaluated by master curve concept
Popis výsledku anglicky
The paper focuses on assessing the usability of fatigue pre-cracked Charpy type specimens when evaluating the resistance of steel with ferritic-pearlitic structure to the initiation of unstable fractures. The suitability of using the specimens is evaluated on the basis of comparing experimentally established values of fracture toughness on pre-cracked Charpy type specimens and the values of this characteristics determined using Compact Tension (CT) specimens. For the evaluation and comparison of the fracture toughness temperature dependences determined on individual specimen types the master curve concept quantifying fracture toughness transition was applied. In the case of the steel employed, very good agreement was found to exist between the characteristics determined on individual types of specimen. It was shown that fracture toughness determined on pre-cracked Charpy type specimens can be regarded as a representative measure of resistance of the material employed to the brittle fracture occurrence.
Klasifikace
Druh
J<sub>ost</sub> - Ostatní články v recenzovaných periodicích
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/LO1202" target="_blank" >LO1202: NETME CENTRE PLUS</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2018
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materiálové inžinierstvo
ISSN
1335-0803
e-ISSN
—
Svazek periodika
24
Číslo periodika v rámci svazku
4
Stát vydavatele periodika
SK - Slovenská republika
Počet stran výsledku
7
Strana od-do
101-107