Nerovnoměrné korozní napadení slitin titanu
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F25794787%3A_____%2F06%3A23" target="_blank" >RIV/25794787:_____/06:23 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Non-uniform corrosion of titanium alloys
Popis výsledku v původním jazyce
A specific problem encountered in stomatology applications of titanium and its alloys is the use of fluoride-containing dental care agents in the prevention of dental ailments. The paper deals with non-uniform corrosion suffered by titanium based materials in fluoride environments. The experimental results indicated that, in most of the systems studied, the alloys are not subject to any non-uniform corrosion attack. Also, the data obtained were used to evaluate the corrosion resistance of the specimensin media having different fluoride concentrations. It has been possible to differentiate, by evaluation of potential-current curves, two distinct modes of impact of the fluorides on the material tested: a mode where the material remains resistant, and another mode where passive film breakdown occurs causing the film to lose its protective properties.
Název v anglickém jazyce
Non-uniform corrosion of titanium alloys
Popis výsledku anglicky
A specific problem encountered in stomatology applications of titanium and its alloys is the use of fluoride-containing dental care agents in the prevention of dental ailments. The paper deals with non-uniform corrosion suffered by titanium based materials in fluoride environments. The experimental results indicated that, in most of the systems studied, the alloys are not subject to any non-uniform corrosion attack. Also, the data obtained were used to evaluate the corrosion resistance of the specimensin media having different fluoride concentrations. It has been possible to differentiate, by evaluation of potential-current curves, two distinct modes of impact of the fluorides on the material tested: a mode where the material remains resistant, and another mode where passive film breakdown occurs causing the film to lose its protective properties.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JK - Koroze a povrchové úpravy materiálu
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2006
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
12th Corrosion Symposium Szczyrk 06
ISBN
0473-7733
ISSN
—
e-ISSN
—
Počet stran výsledku
4
Strana od-do
53-56
Název nakladatele
—
Místo vydání
Szczyrk
Místo konání akce
Szczyrk
Datum konání akce
1. 1. 2006
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—