Accelerated Carbide Spheroidisation of Chromium Bearing Steel by Induction Heating
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F26316919%3A_____%2F13%3A%230000493" target="_blank" >RIV/26316919:_____/13:#0000493 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.scientific.net/AMR.739.161" target="_blank" >http://www.scientific.net/AMR.739.161</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/AMR.739.161" target="_blank" >10.4028/www.scientific.net/AMR.739.161</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Accelerated Carbide Spheroidisation of Chromium Bearing Steel by Induction Heating
Popis výsledku v původním jazyce
Inevitable part of bearing steel processing is soft annealing. Hot formed semi-products usually have unfavorable structure for machining. The lamellar pearlite in semi-products is transformed to globular pearlite by soft annealing. This long-lasting process is usually in practice carried out by annealing in furnace for tens of hours. Furnace processing effectiveness is very often raised by increasing amount of batch mass for one annealing. The time needed for soft annealing is then significantly extended by period necessary for homogeneous heating and slow cooling of the heat. Presented paper shows different way of carbide spheroidisation and steel softening using induction heating of 100CrMnSi6-4 bearing steel. The new process of soft annealing by induction heating is achievable in minutes. This method is appropriate especially for small semi-products and for continuous processes.
Název v anglickém jazyce
Accelerated Carbide Spheroidisation of Chromium Bearing Steel by Induction Heating
Popis výsledku anglicky
Inevitable part of bearing steel processing is soft annealing. Hot formed semi-products usually have unfavorable structure for machining. The lamellar pearlite in semi-products is transformed to globular pearlite by soft annealing. This long-lasting process is usually in practice carried out by annealing in furnace for tens of hours. Furnace processing effectiveness is very often raised by increasing amount of batch mass for one annealing. The time needed for soft annealing is then significantly extended by period necessary for homogeneous heating and slow cooling of the heat. Presented paper shows different way of carbide spheroidisation and steel softening using induction heating of 100CrMnSi6-4 bearing steel. The new process of soft annealing by induction heating is achievable in minutes. This method is appropriate especially for small semi-products and for continuous processes.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED2.1.00%2F03.0077" target="_blank" >ED2.1.00/03.0077: Západočeské materiálově metalurgické centrum</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Advanced Materials Research
ISSN
1662-8985
e-ISSN
—
Svazek periodika
739
Číslo periodika v rámci svazku
08/2013
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
6
Strana od-do
161-166
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—