Thermal expansion evolution of metastable β Ti-15Mo alloy during linear heating
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F26722445%3A_____%2F18%3AN0000074" target="_blank" >RIV/26722445:_____/18:N0000074 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1088/1757-899X/461/1/012094" target="_blank" >http://dx.doi.org/10.1088/1757-899X/461/1/012094</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1088/1757-899X/461/1/012094" target="_blank" >10.1088/1757-899X/461/1/012094</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Thermal expansion evolution of metastable β Ti-15Mo alloy during linear heating
Popis výsledku v původním jazyce
Thermal expansion measurement was employed for characterization of phase transformations occurring in metastable β titanium alloy (Ti-15Mo) during linear heating with three different heating rates. Effects of the transformations on materials dimensions is discussed and compared with changes of lattice parameters of present phases obtained from in-situ powder neutron diffraction. The shrinkage of the material with increasing temperature at about 300 °C was attributed to the decrease of lattice parameter of β phase, which occurs due to diffusion of alloying elements out of ω phase. Complete dissolution of ω phase was detected at 560 °C regardless of the heating rate.
Název v anglickém jazyce
Thermal expansion evolution of metastable β Ti-15Mo alloy during linear heating
Popis výsledku anglicky
Thermal expansion measurement was employed for characterization of phase transformations occurring in metastable β titanium alloy (Ti-15Mo) during linear heating with three different heating rates. Effects of the transformations on materials dimensions is discussed and compared with changes of lattice parameters of present phases obtained from in-situ powder neutron diffraction. The shrinkage of the material with increasing temperature at about 300 °C was attributed to the decrease of lattice parameter of β phase, which occurs due to diffusion of alloying elements out of ω phase. Complete dissolution of ω phase was detected at 560 °C regardless of the heating rate.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2018
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
IOP Conference Series: Materials Science and Engineering, Volume 461, Issue 1, 10 December 2018
ISBN
—
ISSN
1757-8981
e-ISSN
—
Počet stran výsledku
6
Strana od-do
1-6
Název nakladatele
IOP Publishing
Místo vydání
—
Místo konání akce
Plze
Datum konání akce
14. 11. 2018
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—