The use of metallography for examination of causes of surface defects on visual parts
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F46747885%3A24620%2F17%3A00004693" target="_blank" >RIV/46747885:24620/17:00004693 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.scientific.net/SSP.270.107" target="_blank" >https://www.scientific.net/SSP.270.107</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/SSP.270.107" target="_blank" >10.4028/www.scientific.net/SSP.270.107</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
The use of metallography for examination of causes of surface defects on visual parts
Popis výsledku v původním jazyce
Many of currently manufactured components intended for automotive, must not only meet the requirements on functionality, but also considerable demands on the visual appearance. Parts are subjected to thorough inspection and suppliers are forced to deal with causes of a very slight visual defects. When examining the defects, it is necessary to use a whole range of advanced analytical methods and procedures previously used only for identification of the physical and chemical properties and structure of the material. This paper deals with several examples which have been solved. It focuses especially on the use of demanding metallographic sample preparation from components with surface defects, examining the defects on the cross-section using mainly microscopic techniques and determining the causes of their generation. These results then serve as a basis for modification of the technology and thus they are the tool for significant reduction of amount of NOK parts.
Název v anglickém jazyce
The use of metallography for examination of causes of surface defects on visual parts
Popis výsledku anglicky
Many of currently manufactured components intended for automotive, must not only meet the requirements on functionality, but also considerable demands on the visual appearance. Parts are subjected to thorough inspection and suppliers are forced to deal with causes of a very slight visual defects. When examining the defects, it is necessary to use a whole range of advanced analytical methods and procedures previously used only for identification of the physical and chemical properties and structure of the material. This paper deals with several examples which have been solved. It focuses especially on the use of demanding metallographic sample preparation from components with surface defects, examining the defects on the cross-section using mainly microscopic techniques and determining the causes of their generation. These results then serve as a basis for modification of the technology and thus they are the tool for significant reduction of amount of NOK parts.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/LO1201" target="_blank" >LO1201: ROZVOJ ÚSTAVU PRO NANOMATERIÁLY, POKROČILÉ TECHNOLOGIE A INOVACE TECHNICKÉ UNIVERZITY V LIBERCI</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Solid State Phenomena
ISBN
978-303571241-4
ISSN
16629779
e-ISSN
—
Počet stran výsledku
5
Strana od-do
107-111
Název nakladatele
Trans Tech Publications
Místo vydání
—
Místo konání akce
Mariánské Lázně
Datum konání akce
1. 1. 2017
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—