Analysis of thermal and mechanical properties of cable insulations designed for operation under emergency conditions
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F49777513%3A23220%2F12%3A43916079" target="_blank" >RIV/49777513:23220/12:43916079 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Analysis of thermal and mechanical properties of cable insulations designed for operation under emergency conditions
Popis výsledku v původním jazyce
Paper is focused on a comparison of thermo mechanical properties of two plastic insulation materials used for cable sheaths. First measurement was analysed in the temperature range from ambient temperature to 60 °C because of possible laying of the cables during higher temperatures than ambient temperature. Tensile strength and elongation at break were measured by universal testing machine at following temperatures: 22 °C (ambient temperature), 40, 50, 55 and 60 °C. Results show maximum temperatures suitable for laying of the cables. The measurement of softening temperatures of sheathing materials by the thermo mechanical analysis (TMA) followed. It was determined, that recognizable change of properties is coming in the temperature interval from 60 to100 °C, which corresponding with the start of melting. Results from the thermo mechanical analysis in a dynamic mode (DTMA) provide also information about glass transition.
Název v anglickém jazyce
Analysis of thermal and mechanical properties of cable insulations designed for operation under emergency conditions
Popis výsledku anglicky
Paper is focused on a comparison of thermo mechanical properties of two plastic insulation materials used for cable sheaths. First measurement was analysed in the temperature range from ambient temperature to 60 °C because of possible laying of the cables during higher temperatures than ambient temperature. Tensile strength and elongation at break were measured by universal testing machine at following temperatures: 22 °C (ambient temperature), 40, 50, 55 and 60 °C. Results show maximum temperatures suitable for laying of the cables. The measurement of softening temperatures of sheathing materials by the thermo mechanical analysis (TMA) followed. It was determined, that recognizable change of properties is coming in the temperature interval from 60 to100 °C, which corresponding with the start of melting. Results from the thermo mechanical analysis in a dynamic mode (DTMA) provide also information about glass transition.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JA - Elektronika a optoelektronika, elektrotechnika
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED2.1.00%2F03.0094" target="_blank" >ED2.1.00/03.0094: Regionální inovační centrum elektrotechniky (RICE)</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2012
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Annals of DAAAM for 2012 & Proceedings of the 23rd International DAAAM Symposium
ISBN
978-3-901509-91-9
ISSN
2304-1382
e-ISSN
—
Počet stran výsledku
6
Strana od-do
679-684
Název nakladatele
DAAAM International
Místo vydání
Vienna
Místo konání akce
University of Zadar, Zadar, Croatia
Datum konání akce
21. 10. 2012
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—