Impact of thermal modification on the chemical changes and impact bending strength of European oak and Norway spruce wood
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41320%2F19%3A81128" target="_blank" >RIV/60460709:41320/19:81128 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S0263822318334263?via%3Dihub" target="_blank" >https://www.sciencedirect.com/science/article/pii/S0263822318334263?via%3Dihub</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.compstruct.2019.02.091" target="_blank" >10.1016/j.compstruct.2019.02.091</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Impact of thermal modification on the chemical changes and impact bending strength of European oak and Norway spruce wood
Popis výsledku v původním jazyce
This paper deals with the effect of various thermal modification temperatures (160 degrees C, 180 degrees C and 210 degrees C) on changes in the basic chemical components of wood, and the effect of these changes in wood on the impact bending strength (IBS) of European oak (Quercus robur L.) and Norway spruce (Picea abies (L.) H. Karst) wood in comparison with unmodified wood. The IBS was determined according to ISO 13061-10 (2017), and the chemical composition (extractives, lignin, holocellulose, cellulose and hemicelluloses) by NREL methods (wet chemical methods). During the thermal modification the IBS increased in both wood species at first (temperature of 160 degrees C), but at higher temperatures these values gradually decreased. The highest drop in IBS values, found at a temperature of 210 degrees C, was 32,2% for oak and 39,8% for spruce. Thermal modification caused an increase in the relative content of extractives, lignin and cellulose, but the relative content of hemicelluloses in the wood
Název v anglickém jazyce
Impact of thermal modification on the chemical changes and impact bending strength of European oak and Norway spruce wood
Popis výsledku anglicky
This paper deals with the effect of various thermal modification temperatures (160 degrees C, 180 degrees C and 210 degrees C) on changes in the basic chemical components of wood, and the effect of these changes in wood on the impact bending strength (IBS) of European oak (Quercus robur L.) and Norway spruce (Picea abies (L.) H. Karst) wood in comparison with unmodified wood. The IBS was determined according to ISO 13061-10 (2017), and the chemical composition (extractives, lignin, holocellulose, cellulose and hemicelluloses) by NREL methods (wet chemical methods). During the thermal modification the IBS increased in both wood species at first (temperature of 160 degrees C), but at higher temperatures these values gradually decreased. The highest drop in IBS values, found at a temperature of 210 degrees C, was 32,2% for oak and 39,8% for spruce. Thermal modification caused an increase in the relative content of extractives, lignin and cellulose, but the relative content of hemicelluloses in the wood
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
<a href="/cs/project/EF16_019%2F0000803" target="_blank" >EF16_019/0000803: Excelentní Výzkum jako podpora Adaptace lesnictví a dřevařství na globální změnu a 4. průmyslovou revoluci</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2019
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
COMPOSITE STRUCTURES
ISSN
0263-8223
e-ISSN
—
Svazek periodika
216
Číslo periodika v rámci svazku
2019
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
9
Strana od-do
80-88
Kód UT WoS článku
000461162500009
EID výsledku v databázi Scopus
2-s2.0-85062238128