Effect of thermal modification on properties and milling behaviour of African padauk (Pterocarpus soyauxii Taub.) wood
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41320%2F20%3A84752" target="_blank" >RIV/60460709:41320/20:84752 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S2238785420314198" target="_blank" >https://www.sciencedirect.com/science/article/pii/S2238785420314198</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.jmrt.2020.06.018" target="_blank" >10.1016/j.jmrt.2020.06.018</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Effect of thermal modification on properties and milling behaviour of African padauk (Pterocarpus soyauxii Taub.) wood
Popis výsledku v původním jazyce
The purpose of this study was to analyze the effect of thermal treatment on chemical changes, mechanical properties and machining behavior of African padauk wood. Thermal modification of padauk wood was carried out at 3 different temperatures (160 degrees C, 180 degrees, and 210 degrees). Effect of modification temperature on chemical constituents and bending proper-ties of padauk wood were ascertained. Thermally modified and un-modified samples were subjected to milling operation with combination of various processing parameters such as cutting speed (20, 30, 40 m/s), feed speed (4, 8, 11 m/min) and rake angle (15 degrees, 20 degrees, 25 degrees), to obtain the optimum combination in terms superior surface quality (surface roughness and surface waviness) and minimum energy consumption. Cellulose and lignin proportion increased while hemicellulose proportion reduced significantly following thermal modifi-cation. Modification temperature, particularly 210 degrees, had significant effect on the chemica
Název v anglickém jazyce
Effect of thermal modification on properties and milling behaviour of African padauk (Pterocarpus soyauxii Taub.) wood
Popis výsledku anglicky
The purpose of this study was to analyze the effect of thermal treatment on chemical changes, mechanical properties and machining behavior of African padauk wood. Thermal modification of padauk wood was carried out at 3 different temperatures (160 degrees C, 180 degrees, and 210 degrees). Effect of modification temperature on chemical constituents and bending proper-ties of padauk wood were ascertained. Thermally modified and un-modified samples were subjected to milling operation with combination of various processing parameters such as cutting speed (20, 30, 40 m/s), feed speed (4, 8, 11 m/min) and rake angle (15 degrees, 20 degrees, 25 degrees), to obtain the optimum combination in terms superior surface quality (surface roughness and surface waviness) and minimum energy consumption. Cellulose and lignin proportion increased while hemicellulose proportion reduced significantly following thermal modifi-cation. Modification temperature, particularly 210 degrees, had significant effect on the chemica
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
<a href="/cs/project/EF16_019%2F0000803" target="_blank" >EF16_019/0000803: Excelentní Výzkum jako podpora Adaptace lesnictví a dřevařství na globální změnu a 4. průmyslovou revoluci</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2020
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T
ISSN
2238-7854
e-ISSN
—
Svazek periodika
9
Číslo periodika v rámci svazku
4
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
13
Strana od-do
9315-9327
Kód UT WoS článku
000560998500008
EID výsledku v databázi Scopus
2-s2.0-85108633307