Phenol-formaldehyde-resin treatment of Scots pine sapwood for the reduction of resin exudation through coatings
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60460709%3A41320%2F22%3A94146" target="_blank" >RIV/60460709:41320/22:94146 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.tandfonline.com/doi/full/10.1080/17480272.2021.2017479" target="_blank" >https://www.tandfonline.com/doi/full/10.1080/17480272.2021.2017479</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1080/17480272.2021.2017479" target="_blank" >10.1080/17480272.2021.2017479</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Phenol-formaldehyde-resin treatment of Scots pine sapwood for the reduction of resin exudation through coatings
Popis výsledku v původním jazyce
Brown discolouration caused by resin exudation from knots is a problem for a range of light coloured painted pines, and will negatively affect the appearance of the finish. To solve this problem, a hot-and-cold bath impregnation process of wood prior to painting was tested. Sawn timber, 18 x 120 mm in cross-section dimension, were heated in an oven and then immediately immersed in a cold liquid containing a phenol-formaldehyde-based solution, filling a 1-5 mm thick layer beneath the surface with phenol-formaldehyde. After curing, the timbers were painted with a white coloured coating system intended for exterior use, and tested in artificial weathering test (QUV). The phenol-formaldehyde treatment greatly reduced the discolouration of the coating compared to non-impregnated wood.
Název v anglickém jazyce
Phenol-formaldehyde-resin treatment of Scots pine sapwood for the reduction of resin exudation through coatings
Popis výsledku anglicky
Brown discolouration caused by resin exudation from knots is a problem for a range of light coloured painted pines, and will negatively affect the appearance of the finish. To solve this problem, a hot-and-cold bath impregnation process of wood prior to painting was tested. Sawn timber, 18 x 120 mm in cross-section dimension, were heated in an oven and then immediately immersed in a cold liquid containing a phenol-formaldehyde-based solution, filling a 1-5 mm thick layer beneath the surface with phenol-formaldehyde. After curing, the timbers were painted with a white coloured coating system intended for exterior use, and tested in artificial weathering test (QUV). The phenol-formaldehyde treatment greatly reduced the discolouration of the coating compared to non-impregnated wood.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
<a href="/cs/project/EF16_019%2F0000803" target="_blank" >EF16_019/0000803: Excelentní Výzkum jako podpora Adaptace lesnictví a dřevařství na globální změnu a 4. průmyslovou revoluci</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2022
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Wood Material Science and Engineering
ISSN
1748-0272
e-ISSN
—
Svazek periodika
17
Číslo periodika v rámci svazku
2
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
3
Strana od-do
144-146
Kód UT WoS článku
000742230400001
EID výsledku v databázi Scopus
2-s2.0-85122800569