Effect of layered silicates on rheological and mechanical properties and thermal stability of high-molar mass polydimethylsiloxane matrix
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F11%3A43891669" target="_blank" >RIV/60461373:22310/11:43891669 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Effect of layered silicates on rheological and mechanical properties and thermal stability of high-molar mass polydimethylsiloxane matrix
Popis výsledku v původním jazyce
The effect of surface modified fillers based on montmorillonite on rheological and mechanical properties and thermal stability of high-molar mass polydimethylsiloxane matrix was evaluated. Silicone rubber/clay composites were prepared via homogenisationon open two roll-mill followed by torque measurement at two different temperatures. At 30 degrees C and 100 degrees C the torque did not extremely differ excepting the mixtures containing Cloisite 15A where it achieved the maximum at 3 phr montmorillonite content, but the tensile strength reached the similar values in all mixtures. Thermogravimetric analysis was utilized to find out the differences in weight decay of composites in silicone rubber/montmorillonite mixtures and in unfilled silicone rubber.Synergism of fillers was also studied and led to tensile strength increase.
Název v anglickém jazyce
Effect of layered silicates on rheological and mechanical properties and thermal stability of high-molar mass polydimethylsiloxane matrix
Popis výsledku anglicky
The effect of surface modified fillers based on montmorillonite on rheological and mechanical properties and thermal stability of high-molar mass polydimethylsiloxane matrix was evaluated. Silicone rubber/clay composites were prepared via homogenisationon open two roll-mill followed by torque measurement at two different temperatures. At 30 degrees C and 100 degrees C the torque did not extremely differ excepting the mixtures containing Cloisite 15A where it achieved the maximum at 3 phr montmorillonite content, but the tensile strength reached the similar values in all mixtures. Thermogravimetric analysis was utilized to find out the differences in weight decay of composites in silicone rubber/montmorillonite mixtures and in unfilled silicone rubber.Synergism of fillers was also studied and led to tensile strength increase.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2011
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
e-Polymers
ISSN
1618-7229
e-ISSN
—
Svazek periodika
2011
Číslo periodika v rámci svazku
91
Stát vydavatele periodika
FR - Francouzská republika
Počet stran výsledku
8
Strana od-do
1-8
Kód UT WoS článku
000294945400002
EID výsledku v databázi Scopus
—