Properties of rubber filled with montmorillonite with various surface modifications
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61389013%3A_____%2F12%3A00380463" target="_blank" >RIV/61389013:_____/12:00380463 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1002/pat.2060" target="_blank" >http://dx.doi.org/10.1002/pat.2060</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1002/pat.2060" target="_blank" >10.1002/pat.2060</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Properties of rubber filled with montmorillonite with various surface modifications
Popis výsledku v původním jazyce
Layered silicate/natural rubber composites were prepared by direct polymer melt intercalation. Na-montmorillonite Kunipia-F and its organic derivates (organo-clays) prepared by ion exchange were used as clay fillers. Silica (SiO2)Ultrasil VN3, a filler commonly used in the rubber industry, was used in combination with clay fillers. The effect of clay or organo-clay loading from 1 up to 10 phr without (0 phr) or with silica (15 phr) showed significant improvement of the tensile properties (stress at break, strain at break and modulus M100). Modification of montmorillonite by three alkylammonium cations with the same length of alkylammonium chain (18 carbons) and different structure resulted in altered reinforcing and plasticizing effects of the filler in composites with rubber matrix.
Název v anglickém jazyce
Properties of rubber filled with montmorillonite with various surface modifications
Popis výsledku anglicky
Layered silicate/natural rubber composites were prepared by direct polymer melt intercalation. Na-montmorillonite Kunipia-F and its organic derivates (organo-clays) prepared by ion exchange were used as clay fillers. Silica (SiO2)Ultrasil VN3, a filler commonly used in the rubber industry, was used in combination with clay fillers. The effect of clay or organo-clay loading from 1 up to 10 phr without (0 phr) or with silica (15 phr) showed significant improvement of the tensile properties (stress at break, strain at break and modulus M100). Modification of montmorillonite by three alkylammonium cations with the same length of alkylammonium chain (18 carbons) and different structure resulted in altered reinforcing and plasticizing effects of the filler in composites with rubber matrix.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2012
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Polymers for Advanced Technologies
ISSN
1042-7147
e-ISSN
—
Svazek periodika
23
Číslo periodika v rámci svazku
10
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
8
Strana od-do
1414-1421
Kód UT WoS článku
000308876500011
EID výsledku v databázi Scopus
—