Swelling and pillaring of the layered precursor IPC-1P: tiny details determine everything
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61388955%3A_____%2F14%3A00446859" target="_blank" >RIV/61388955:_____/14:00446859 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1039/c4dt00165f" target="_blank" >http://dx.doi.org/10.1039/c4dt00165f</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1039/c4dt00165f" target="_blank" >10.1039/c4dt00165f</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Swelling and pillaring of the layered precursor IPC-1P: tiny details determine everything
Popis výsledku v původním jazyce
The influence of swelling (i.e. the size of tetraalkylammonium surfactant molecule, the presence of tetrapropylammonium hydroxide (TPAOH), pH) and pillaring (i. e. the ratio between the swollen precursor IPC-1P and tetraethyl orthosilicate) conditions onthe structure and textural properties of the resulting materials was studied in detail for IPC-1P, which is the layered precursor of zeolite PCR. The swelling of IPC-1P proceeds efficiently under basic conditions both in mixed CnH2n+N-1(CH3)(3)Cl/TPAOHsystems and in CnH2n+N-1(CH3)(3)OH (n = 8, 10, 12, 14, 16, 18) solutions at pH = 13-14. The intercalation of CnH2n+1N+(CH3) 3 in IPC-1P resulted in the formation of expanded materials with interlayer distances growing with increasing length of the alkylchain in CnH2n+N-1(CH3)(3) +: 1.59-1.86 (n = 8) < 1.89-2.11 (10) < 2.05-2.26 (12) = 2.08-2.26 (14) < 2.37-2.43 (16) < 2.57-2.71 (18) angstrom. IPC-2 zeolite was formed during calcination of IPC-1P samples swollen in CnH2n+1N(CH3) 3OH solu
Název v anglickém jazyce
Swelling and pillaring of the layered precursor IPC-1P: tiny details determine everything
Popis výsledku anglicky
The influence of swelling (i.e. the size of tetraalkylammonium surfactant molecule, the presence of tetrapropylammonium hydroxide (TPAOH), pH) and pillaring (i. e. the ratio between the swollen precursor IPC-1P and tetraethyl orthosilicate) conditions onthe structure and textural properties of the resulting materials was studied in detail for IPC-1P, which is the layered precursor of zeolite PCR. The swelling of IPC-1P proceeds efficiently under basic conditions both in mixed CnH2n+N-1(CH3)(3)Cl/TPAOHsystems and in CnH2n+N-1(CH3)(3)OH (n = 8, 10, 12, 14, 16, 18) solutions at pH = 13-14. The intercalation of CnH2n+1N+(CH3) 3 in IPC-1P resulted in the formation of expanded materials with interlayer distances growing with increasing length of the alkylchain in CnH2n+N-1(CH3)(3) +: 1.59-1.86 (n = 8) < 1.89-2.11 (10) < 2.05-2.26 (12) = 2.08-2.26 (14) < 2.37-2.43 (16) < 2.57-2.71 (18) angstrom. IPC-2 zeolite was formed during calcination of IPC-1P samples swollen in CnH2n+1N(CH3) 3OH solu
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CF - Fyzikální chemie a teoretická chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GP13-17593P" target="_blank" >GP13-17593P: Využití nových organických templátů pro syntézu zeolitů</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Dalton Transactions
ISSN
1477-9226
e-ISSN
—
Svazek periodika
43
Číslo periodika v rámci svazku
27
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
10
Strana od-do
10548-10557
Kód UT WoS článku
000338117200027
EID výsledku v databázi Scopus
2-s2.0-84902668602