Influence of Flat Cavity Formation on Stress vs. Strain and Strain-Rate Relations of Superplastic Deformation in 3Y-TZP
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61389005%3A_____%2F10%3A00346945" target="_blank" >RIV/61389005:_____/10:00346945 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Influence of Flat Cavity Formation on Stress vs. Strain and Strain-Rate Relations of Superplastic Deformation in 3Y-TZP
Popis výsledku v původním jazyce
During superplastic deformation (SPD) of tetragonal zirconia polycrystals containing 3 mol% yttria (3Y-TZP) at high strain-rates, a number of crack-like flat cavities having very narrow gaps lying along grain boundaries mostly normal to the tensile axisare produced in addition to conventional cavities. In order to see when (from which strain point) the flat cavities get started to form, the tensile deformation of the 3Y-TZP was interrupted at different strain points including a yield point, and then asmall angle neutron scattering (SANS) technique was applied to examine the existence of the flat cavities. It was found that no flat cavities were produced at the yield point but they got started to form soon after the yielding, i.e., after a superplastic flow began. The formation of the flat cavities can decrease the cross-sectional area of the specimen, resulting in a decrease in the flow stress apparently.
Název v anglickém jazyce
Influence of Flat Cavity Formation on Stress vs. Strain and Strain-Rate Relations of Superplastic Deformation in 3Y-TZP
Popis výsledku anglicky
During superplastic deformation (SPD) of tetragonal zirconia polycrystals containing 3 mol% yttria (3Y-TZP) at high strain-rates, a number of crack-like flat cavities having very narrow gaps lying along grain boundaries mostly normal to the tensile axisare produced in addition to conventional cavities. In order to see when (from which strain point) the flat cavities get started to form, the tensile deformation of the 3Y-TZP was interrupted at different strain points including a yield point, and then asmall angle neutron scattering (SANS) technique was applied to examine the existence of the flat cavities. It was found that no flat cavities were produced at the yield point but they got started to form soon after the yielding, i.e., after a superplastic flow began. The formation of the flat cavities can decrease the cross-sectional area of the specimen, resulting in a decrease in the flow stress apparently.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BG - Jaderná, atomová a molekulová fyzika, urychlovače
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2010
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials Transactions
ISSN
1345-9678
e-ISSN
—
Svazek periodika
51
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
JP - Japonsko
Počet stran výsledku
7
Strana od-do
—
Kód UT WoS článku
000276967200025
EID výsledku v databázi Scopus
—