Crack growth in conventionally manufactured pure nickel, titanium and aluminum and the cold spray additively manufactured equivalents
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61389021%3A_____%2F22%3A00558574" target="_blank" >RIV/61389021:_____/22:00558574 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68407700:21340/22:00371001
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S2772369022000184?via%3Dihub" target="_blank" >https://www.sciencedirect.com/science/article/pii/S2772369022000184?via%3Dihub</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.addlet.2022.100043" target="_blank" >10.1016/j.addlet.2022.100043</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Crack growth in conventionally manufactured pure nickel, titanium and aluminum and the cold spray additively manufactured equivalents
Popis výsledku v původním jazyce
It has recently been shown that when the da/dN versus ΔK curves associated with crack growth in conventionally manufactured, additively manufactured (AM), and cold spray additively manufactured (CSAM) 316L stainless steel are replotted with da/dN expressed as a function of the Schwalbe crack driving force (Δκ), then the various different curves collapsed onto a single master curve. This study reveals that this phenomenon also arises for crack growth in titanium, nickel, and aluminum. In each case, the da/dN versus Δκ relationship is shown to be independent of whether the specimen was conventionally manufactured or produced by CSAM.
Název v anglickém jazyce
Crack growth in conventionally manufactured pure nickel, titanium and aluminum and the cold spray additively manufactured equivalents
Popis výsledku anglicky
It has recently been shown that when the da/dN versus ΔK curves associated with crack growth in conventionally manufactured, additively manufactured (AM), and cold spray additively manufactured (CSAM) 316L stainless steel are replotted with da/dN expressed as a function of the Schwalbe crack driving force (Δκ), then the various different curves collapsed onto a single master curve. This study reveals that this phenomenon also arises for crack growth in titanium, nickel, and aluminum. In each case, the da/dN versus Δκ relationship is shown to be independent of whether the specimen was conventionally manufactured or produced by CSAM.
Klasifikace
Druh
J<sub>ost</sub> - Ostatní články v recenzovaných periodicích
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2022
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Additive Manufacturing Letters
ISSN
2772-3690
e-ISSN
—
Svazek periodika
2
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
6
Strana od-do
100043
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—