Distribution of impurities in directionally solidified samples with planar crystallization front
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F09%3A00022132" target="_blank" >RIV/61989100:27360/09:00022132 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Distribution of impurities in directionally solidified samples with planar crystallization front
Popis výsledku v původním jazyce
Method of directionally controlled solidification with planar crystallization front is used, as a rule, to purify the main component of impurities. It is considered that distribution of each impurity component along the length of directionally solidifiedsample with planar front is predetermined by the value of the equilibrium distribution coefficient (K) of each impurity with the main component. The K value is determined from equilibrium binary phase diagram as the relation K = CS / CL, where CS and CLare contents of the impurity under examination in coexisting solid and liquid phases. On condition that DS = 0 and DL = infinity and K < 1, at crystallization with planar front the impurity content along the length of the directionally solidified sampleincreases constantly and reaches maximum in the last part of the sample. In case of the value K > 1 the impurity content on the contrary decreases from the initial part of the sample to the final one.
Název v anglickém jazyce
Distribution of impurities in directionally solidified samples with planar crystallization front
Popis výsledku anglicky
Method of directionally controlled solidification with planar crystallization front is used, as a rule, to purify the main component of impurities. It is considered that distribution of each impurity component along the length of directionally solidifiedsample with planar front is predetermined by the value of the equilibrium distribution coefficient (K) of each impurity with the main component. The K value is determined from equilibrium binary phase diagram as the relation K = CS / CL, where CS and CLare contents of the impurity under examination in coexisting solid and liquid phases. On condition that DS = 0 and DL = infinity and K < 1, at crystallization with planar front the impurity content along the length of the directionally solidified sampleincreases constantly and reaches maximum in the last part of the sample. In case of the value K > 1 the impurity content on the contrary decreases from the initial part of the sample to the final one.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2009
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Hutnické listy
ISSN
0018-8069
e-ISSN
—
Svazek periodika
62
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
8
Strana od-do
—
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—