On the distribution of directionally solidified samples with a planar crystallization front
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F09%3A00022139" target="_blank" >RIV/61989100:27360/09:00022139 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
On the distribution of directionally solidified samples with a planar crystallization front
Popis výsledku v původním jazyce
Method of directionally controlled solidification with planar crystallization front is used, as a rule, to purify the main component of impurities. It is considered that distribution of each impurity component along the length of directionally solidifiedsample with planar front is predetermined by the value of the equilibrium distribution coefficient (K) of each impurity with the main component. The K value is determined from equilibrium binary phase diagram as the relation K = CS / CL, where CS and CLare contents of the impurity under examination in coexisting solid and liquid phases. On condition that DS = 0 and DL = infinity and K < 1, at crystallization with planar front the impurity content along the length of the directionally solidified sampleincreases constantly and reaches maximum in the last part of the sample. In case of the value K > 1 the impurity content on the contrary decreases from the initial part of the sample to the final one.
Název v anglickém jazyce
On the distribution of directionally solidified samples with a planar crystallization front
Popis výsledku anglicky
Method of directionally controlled solidification with planar crystallization front is used, as a rule, to purify the main component of impurities. It is considered that distribution of each impurity component along the length of directionally solidifiedsample with planar front is predetermined by the value of the equilibrium distribution coefficient (K) of each impurity with the main component. The K value is determined from equilibrium binary phase diagram as the relation K = CS / CL, where CS and CLare contents of the impurity under examination in coexisting solid and liquid phases. On condition that DS = 0 and DL = infinity and K < 1, at crystallization with planar front the impurity content along the length of the directionally solidified sampleincreases constantly and reaches maximum in the last part of the sample. In case of the value K > 1 the impurity content on the contrary decreases from the initial part of the sample to the final one.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2009
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
18. International Conference on Metallurgy and Materials METAL 2009
ISBN
978-80-87294-10-9
ISSN
—
e-ISSN
—
Počet stran výsledku
9
Strana od-do
—
Název nakladatele
TANGER, spol. s r.o.
Místo vydání
Ostrava
Místo konání akce
Hradec nad Moravicí
Datum konání akce
19. 5. 2009
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—