Hydrogen treatment of titanium based alloys
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F17%3A10237734" target="_blank" >RIV/61989100:27360/17:10237734 - isvavai.cz</a>
Výsledek na webu
<a href="http://iopscience.iop.org/article/10.1088/1757-899X/266/1/012007/pdf" target="_blank" >http://iopscience.iop.org/article/10.1088/1757-899X/266/1/012007/pdf</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1088/1757-899X/266/1/012007" target="_blank" >10.1088/1757-899X/266/1/012007</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Hydrogen treatment of titanium based alloys
Popis výsledku v původním jazyce
The positive effect of the hydrogen on hot deformation behaviour at 700 and 750 °C was investigated after thermal hydrogen treatment of Ti6Al4V and Ti26Nb alloys. Comparing the results obtained for the non-hydrogenated and hydrogenated specimens of both alloys, it was found that the hydrogen content as high as 1325 wt. ppm has an obvious benefit effect on high temperature deformation behaviour in the Ti6Al4V alloy by stabilizing beta phase and lowering thermal deformation resistance. In the case of Ti26Nb alloy the hydrogen content of 2572 wt. ppm suppressed stress instabilities during hot compression but slightly increased thermal deformation resistance. The microstructure study was performed before and after the isothermal compression tests on the specimens in hydrogenated as well as in non-hydrogenated condition. The hydrogen amounts in the specimens were measured by means of an analyser LECO RH600.
Název v anglickém jazyce
Hydrogen treatment of titanium based alloys
Popis výsledku anglicky
The positive effect of the hydrogen on hot deformation behaviour at 700 and 750 °C was investigated after thermal hydrogen treatment of Ti6Al4V and Ti26Nb alloys. Comparing the results obtained for the non-hydrogenated and hydrogenated specimens of both alloys, it was found that the hydrogen content as high as 1325 wt. ppm has an obvious benefit effect on high temperature deformation behaviour in the Ti6Al4V alloy by stabilizing beta phase and lowering thermal deformation resistance. In the case of Ti26Nb alloy the hydrogen content of 2572 wt. ppm suppressed stress instabilities during hot compression but slightly increased thermal deformation resistance. The microstructure study was performed before and after the isothermal compression tests on the specimens in hydrogenated as well as in non-hydrogenated condition. The hydrogen amounts in the specimens were measured by means of an analyser LECO RH600.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/LO1203" target="_blank" >LO1203: Regionální materiálově technologické výzkumné centrum - Program udržitelnosti</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
IOP Conference Series: Materials Science and Engineering. Volume 266
ISBN
—
ISSN
1757-8981
e-ISSN
1757-899X
Počet stran výsledku
7
Strana od-do
1-7
Název nakladatele
Institute of Physics
Místo vydání
London
Místo konání akce
Kežmarské Žľaby
Datum konání akce
4. 9. 2017
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000419228900007