Design Against Brittle of Elastic-Plastic Fracture of Nuclear Waste Container.
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F03%3A07033085" target="_blank" >RIV/68081723:_____/03:07033085 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Design Against Brittle of Elastic-Plastic Fracture of Nuclear Waste Container.
Popis výsledku v původním jazyce
Design against brittle or elastic plastic fracture of nuclear waste container is discussed based on three different concepts:(i)reserve of ductility defined by means of reference temperature,(ii)deterministic design using linear or elasto-plastic fracture mechanics associated with reserve factors,and (iii)probabilistic design associated with RCC-MR failure assessment diagram. Cast ferritic steel predetermined for containers of spent nuclear fuel has been used in experimental part of the study.Fracture toughness characteristics necessary for considerations have been obtained by standard 1T three point bend specimens tested statically at different temperatures.Pre-cracked Charpy type specimen has been also employed for the investigations tested statically and dynamically.Material properties necessary for the concept presented are corresponding Master Curve and Weibull distribution of fracture toughness.Special attention has been paid to dynamic loading.Large scatter in reserve factor was
Název v anglickém jazyce
Design Against Brittle of Elastic-Plastic Fracture of Nuclear Waste Container.
Popis výsledku anglicky
Design against brittle or elastic plastic fracture of nuclear waste container is discussed based on three different concepts:(i)reserve of ductility defined by means of reference temperature,(ii)deterministic design using linear or elasto-plastic fracture mechanics associated with reserve factors,and (iii)probabilistic design associated with RCC-MR failure assessment diagram. Cast ferritic steel predetermined for containers of spent nuclear fuel has been used in experimental part of the study.Fracture toughness characteristics necessary for considerations have been obtained by standard 1T three point bend specimens tested statically at different temperatures.Pre-cracked Charpy type specimen has been also employed for the investigations tested statically and dynamically.Material properties necessary for the concept presented are corresponding Master Curve and Weibull distribution of fracture toughness.Special attention has been paid to dynamic loading.Large scatter in reserve factor was
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JL - Únava materiálu a lomová mechanika
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ME%20303" target="_blank" >ME 303: Lomová odolnost ocelí pro kontejnery vyhořelého jaderného paliva</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2003
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
International Conference on STRUCTURAL MECHANICS IN REACTOR TECHNOLOGY /17./.
ISBN
—
ISSN
—
e-ISSN
—
Počet stran výsledku
4
Strana od-do
—
Název nakladatele
International Association for Structural Mechanics in Reactor Technology
Místo vydání
Praha
Místo konání akce
Praha [CZ]
Datum konání akce
17. 8. 2003
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—