Fatigue lifetime estimation of railway axles
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F17%3A00481281" target="_blank" >RIV/68081723:_____/17:00481281 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/00216305:26210/17:PU140214
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.engfailanal.2016.12.014" target="_blank" >http://dx.doi.org/10.1016/j.engfailanal.2016.12.014</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.engfailanal.2016.12.014" target="_blank" >10.1016/j.engfailanal.2016.12.014</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Fatigue lifetime estimation of railway axles
Popis výsledku v původním jazyce
The railway axles are subjected to cyclic loading during their operation. Their load is of long-nterm nature, therefore a real risk of fatigue failure exists. This failure could lead to derailmentnof the whole train with serious consequences. To prevent such scenario, the railway axles havento be safely removed from operation before their final failure occurs.nThis paper presents methodology for the residual fatigue lifetime prediction of the railway axlenbased on the linear elastic fracture mechanics concept. The methodology contains estimation ofnthe critical position of initial crack, prediction of the fatigue crack front shape developmentnduring crack propagation, separation of the bending and press-fitting contributions to thenaxle load, experimental measurement of the crack growth kinetics of EA4T steel and subse-nquent estimation of the residual fatigue lifetime of railway axle. Part of the presented studynis also devoted to the probability aspects of determination of material characteristics describingnfatigue crack propagation and retardation effects caused by existence of plastic zone ahead ofnpropagating fatigue crack. Described methodology is already applied in the design process ofnnew railway axles in Bonatrans company.
Název v anglickém jazyce
Fatigue lifetime estimation of railway axles
Popis výsledku anglicky
The railway axles are subjected to cyclic loading during their operation. Their load is of long-nterm nature, therefore a real risk of fatigue failure exists. This failure could lead to derailmentnof the whole train with serious consequences. To prevent such scenario, the railway axles havento be safely removed from operation before their final failure occurs.nThis paper presents methodology for the residual fatigue lifetime prediction of the railway axlenbased on the linear elastic fracture mechanics concept. The methodology contains estimation ofnthe critical position of initial crack, prediction of the fatigue crack front shape developmentnduring crack propagation, separation of the bending and press-fitting contributions to thenaxle load, experimental measurement of the crack growth kinetics of EA4T steel and subse-nquent estimation of the residual fatigue lifetime of railway axle. Part of the presented studynis also devoted to the probability aspects of determination of material characteristics describingnfatigue crack propagation and retardation effects caused by existence of plastic zone ahead ofnpropagating fatigue crack. Described methodology is already applied in the design process ofnnew railway axles in Bonatrans company.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20306 - Audio engineering, reliability analysis
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Engineering Failure Analysis
ISSN
1350-6307
e-ISSN
—
Svazek periodika
73
Číslo periodika v rámci svazku
MAR
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
19
Strana od-do
139-157
Kód UT WoS článku
000396773100011
EID výsledku v databázi Scopus
2-s2.0-85008414312