Performance of YAG:Ce Scintillators for Low-Energy Electron Detectors in S(T)EM
Popis výsledku v původním jazyce
Cerium activated single crystals of yttrium aluminium garnet (YAG:Ce) Y3-xCexAl5O12 are widely used as scintillators in electron detectors for S(T)EM. Nowadays, it is sometimes necessary to detect low-energy electrons without post-acceleration. In such cases, extremely sensitive detectors are required that are able to detect even electrons with energies of only hundreds of eV while avoiding charging of the scintillator surface. However, commonly used scintillators strongly lose their light yield with the decrease of the incident electron energy. Moreover, a thinner conductive layer on the scintillator surface has to be used to allow low-energy electrons to pass through. Possible charging of the surface negatively affects its cathodoluminescence (CL) light yield. The low-energy electron excitation takes place closer to the scintillator surface where damage can be expected owing to its preparation, which also reduces the CL light yield. The aim was to study the influence of the scintilla
Název v anglickém jazyce
Performance of YAG:Ce Scintillators for Low-Energy Electron Detectors in S(T)EM
Popis výsledku anglicky
Cerium activated single crystals of yttrium aluminium garnet (YAG:Ce) Y3-xCexAl5O12 are widely used as scintillators in electron detectors for S(T)EM. Nowadays, it is sometimes necessary to detect low-energy electrons without post-acceleration. In such cases, extremely sensitive detectors are required that are able to detect even electrons with energies of only hundreds of eV while avoiding charging of the scintillator surface. However, commonly used scintillators strongly lose their light yield with the decrease of the incident electron energy. Moreover, a thinner conductive layer on the scintillator surface has to be used to allow low-energy electrons to pass through. Possible charging of the surface negatively affects its cathodoluminescence (CL) light yield. The low-energy electron excitation takes place closer to the scintillator surface where damage can be expected owing to its preparation, which also reduces the CL light yield. The aim was to study the influence of the scintilla
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JA - Elektronika a optoelektronika, elektrotechnika
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
18th International Microscopy Congres. Proceedings
ISBN
978-80-260-6720-7
ISSN
—
e-ISSN
—
Počet stran výsledku
2
Strana od-do
—
Název nakladatele
Czechoslovak Microscopy Society
Místo vydání
Praha
Místo konání akce
Praha
Datum konání akce
7. 9. 2014
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—