Far infrared and Raman response in tetragonal PZT ceramic films
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F15%3A00454637" target="_blank" >RIV/68378271:_____/15:00454637 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.bsecv.2015.11.003" target="_blank" >http://dx.doi.org/10.1016/j.bsecv.2015.11.003</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.bsecv.2015.11.003" target="_blank" >10.1016/j.bsecv.2015.11.003</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Far infrared and Raman response in tetragonal PZT ceramic films
Popis výsledku v původním jazyce
PbZr0.38Ti0.62O3 and PbZr0.36Ti0.64O3 thick films deposited by screen printing on (0001) single crystal sapphire substrates and prepared at two different sintering temperatures, were studied by Fourier-transform infrared reflectivity, time-domain THz transmission spectroscopy and micro-Raman spectroscopy. The dielectric response is discussed using the Lichtenecker model to account for the porosity of the films and to obtain the dense bulk dielectric functions. Results are compared with bulk tetragonal PZT 42/58 ceramics. The dynamic response in the films is dominated by an overdamped lead-based vibration in the THz range, as known in PZT, but its evaluated dielectric contribution is affected by the porosity and roughness of the surface.
Název v anglickém jazyce
Far infrared and Raman response in tetragonal PZT ceramic films
Popis výsledku anglicky
PbZr0.38Ti0.62O3 and PbZr0.36Ti0.64O3 thick films deposited by screen printing on (0001) single crystal sapphire substrates and prepared at two different sintering temperatures, were studied by Fourier-transform infrared reflectivity, time-domain THz transmission spectroscopy and micro-Raman spectroscopy. The dielectric response is discussed using the Lichtenecker model to account for the porosity of the films and to obtain the dense bulk dielectric functions. Results are compared with bulk tetragonal PZT 42/58 ceramics. The dynamic response in the films is dominated by an overdamped lead-based vibration in the THz range, as known in PZT, but its evaluated dielectric contribution is affected by the porosity and roughness of the surface.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GA14-25639S" target="_blank" >GA14-25639S: Ladění terahertzové odezvy dielektrických materiálů a metamateriálových struktur</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Boletin de la Sociedad Espanola de Ceramica Y Vidrio
ISSN
0366-3175
e-ISSN
—
Svazek periodika
54
Číslo periodika v rámci svazku
6
Stát vydavatele periodika
ES - Španělské království
Počet stran výsledku
6
Strana od-do
219-224
Kód UT WoS článku
000366666700001
EID výsledku v databázi Scopus
2-s2.0-84949568671