Comparison of different methods for assessing the pozzolanic activity of fly ash and bottom ash
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21110%2F23%3A00375872" target="_blank" >RIV/68407700:21110/23:00375872 - isvavai.cz</a>
Výsledek na webu
<a href="https://doi.org/10.1063/5.0137066" target="_blank" >https://doi.org/10.1063/5.0137066</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1063/5.0137066" target="_blank" >10.1063/5.0137066</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Comparison of different methods for assessing the pozzolanic activity of fly ash and bottom ash
Popis výsledku v původním jazyce
The work deals with the comparison of pozzolanic activity of selected fly ash (FA) and bottom ash (BA) from lignite power plants in the Czech Republic. Pozzolanic activity was determined by Frattini test, electrical conductivity test and strength activity index (SAI). The results of the Frattini test performed after 8 days according to CSN EN 196-5 showed that all ashes have pozzolanic activity. In addition, the electrical conductivity test shows significant differences in the reactivity of the ash during the first hours of hydration. SAI was determined on mortars with 25 % ash replacement for cement after 28 days of hydration. The results of pozzolanic activity test methods were compared with each other and the correlations of the methods are discussed.
Název v anglickém jazyce
Comparison of different methods for assessing the pozzolanic activity of fly ash and bottom ash
Popis výsledku anglicky
The work deals with the comparison of pozzolanic activity of selected fly ash (FA) and bottom ash (BA) from lignite power plants in the Czech Republic. Pozzolanic activity was determined by Frattini test, electrical conductivity test and strength activity index (SAI). The results of the Frattini test performed after 8 days according to CSN EN 196-5 showed that all ashes have pozzolanic activity. In addition, the electrical conductivity test shows significant differences in the reactivity of the ash during the first hours of hydration. SAI was determined on mortars with 25 % ash replacement for cement after 28 days of hydration. The results of pozzolanic activity test methods were compared with each other and the correlations of the methods are discussed.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/FW01010195" target="_blank" >FW01010195: Pokročilé výrobní technologie pro strategické využití a skladování vedlejších energetických produktů (VEP)</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2023
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
18th International Conference on Special Concrete and Composites 2021
ISBN
—
ISSN
0094-243X
e-ISSN
—
Počet stran výsledku
8
Strana od-do
1-8
Název nakladatele
AIP Conference Proceedings
Místo vydání
New York
Místo konání akce
Skalsky Dvur
Datum konání akce
13. 10. 2021
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—