Determination of Crack Healing Efficiency of Concrete Containing Crystalline Admixture in Experimental Procedures Using Image Analysis
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21110%2F24%3A00373824" target="_blank" >RIV/68407700:21110/24:00373824 - isvavai.cz</a>
Výsledek na webu
<a href="https://link.springer.com/chapter/10.1007/978-3-031-44603-0_8" target="_blank" >https://link.springer.com/chapter/10.1007/978-3-031-44603-0_8</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1007/978-3-031-44603-0_8" target="_blank" >10.1007/978-3-031-44603-0_8</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Determination of Crack Healing Efficiency of Concrete Containing Crystalline Admixture in Experimental Procedures Using Image Analysis
Popis výsledku v původním jazyce
Crystalline admixtures are often used as waterproofing agents added in the concrete mixture and have the capability of promoting self-healing of concrete. Sika WT-200 P is one of the examples of crystalline admixture typically used at 0.8–2% by cement mass. In this paper, concrete test specimens containing crystalline admixture were cracked using two methods and exposed to different environmental conditions then analysed for crack healing ability using image analysis done through in-house code. Self-healing is visible within the first 7 days of hardening in the test specimens immersed fully in water. After 100 days, images are taken using a Canon camera. The images are converted into grayscale then binary images are produced which show that self-healing has occurred, and the average crack width has been reduced by as much as 90% in some cases. The compressive strength of these specimens is as high as 90 MPa beyond 100 days of self-healing tests.
Název v anglickém jazyce
Determination of Crack Healing Efficiency of Concrete Containing Crystalline Admixture in Experimental Procedures Using Image Analysis
Popis výsledku anglicky
Crystalline admixtures are often used as waterproofing agents added in the concrete mixture and have the capability of promoting self-healing of concrete. Sika WT-200 P is one of the examples of crystalline admixture typically used at 0.8–2% by cement mass. In this paper, concrete test specimens containing crystalline admixture were cracked using two methods and exposed to different environmental conditions then analysed for crack healing ability using image analysis done through in-house code. Self-healing is visible within the first 7 days of hardening in the test specimens immersed fully in water. After 100 days, images are taken using a Canon camera. The images are converted into grayscale then binary images are produced which show that self-healing has occurred, and the average crack width has been reduced by as much as 90% in some cases. The compressive strength of these specimens is as high as 90 MPa beyond 100 days of self-healing tests.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20101 - Civil engineering
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2024
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Lecture Notes in Civil Engineering
ISBN
978-3-031-44603-0
ISSN
2366-2557
e-ISSN
2366-2565
Počet stran výsledku
10
Strana od-do
89-98
Název nakladatele
Springer Nature
Místo vydání
—
Místo konání akce
Vilnius
Datum konání akce
5. 10. 2023
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—