Modifikace oceli vápníkem při plynulém odlévání oceli
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F06%3A00014116" target="_blank" >RIV/61989100:27360/06:00014116 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Modification of Steel by Calcium at Continous Casting of Steel
Popis výsledku v původním jazyce
Making of its and its treatment is always accompanied by formation of non-metallic inclusions as it is impossible to prevent it fully. The efforts are aimed at determination of conditions which cause partial prohibition of their formation or modify themto less harmful inclusions. Formation of inclusions depends on manner of making and treatment of steel, on chemical composition and on technological conditions of their origin. One of the most noxious inclusion is Al2O3 namely due to the fact that it causes clogging of nozzles.Treatment of steel by calcium is efficient method that is used for transformation of aluminium oxide inclusions in steel to less detrimental inclusions, which can have positive influence on steel properties. Transformation of solid aggregations of Al2O3 on liquid calcium aluminate with use of calcium is the most commonly used technology for prevention of clogging of CCM nozzles at casting of aluminium killed steels. Treatment of steel by calcium is also crucial me
Název v anglickém jazyce
Modification of Steel by Calcium at Continous Casting of Steel
Popis výsledku anglicky
Making of its and its treatment is always accompanied by formation of non-metallic inclusions as it is impossible to prevent it fully. The efforts are aimed at determination of conditions which cause partial prohibition of their formation or modify themto less harmful inclusions. Formation of inclusions depends on manner of making and treatment of steel, on chemical composition and on technological conditions of their origin. One of the most noxious inclusion is Al2O3 namely due to the fact that it causes clogging of nozzles.Treatment of steel by calcium is efficient method that is used for transformation of aluminium oxide inclusions in steel to less detrimental inclusions, which can have positive influence on steel properties. Transformation of solid aggregations of Al2O3 on liquid calcium aluminate with use of calcium is the most commonly used technology for prevention of clogging of CCM nozzles at casting of aluminium killed steels. Treatment of steel by calcium is also crucial me
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GA106%2F04%2F0029" target="_blank" >GA106/04/0029: Řízení vlastností tekuté oceli před jejím plynulým odléváním s cílem minimalizovat vady předlitku</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2006
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
13. Internationaler Studententag der Metallurgie
ISBN
3-901384-18-9
ISSN
—
e-ISSN
—
Počet stran výsledku
9
Strana od-do
138-146
Název nakladatele
ASMET, Austrian Society for Metallurgy and Materials
Místo vydání
Leoben
Místo konání akce
—
Datum konání akce
—
Typ akce podle státní příslušnosti
—
Kód UT WoS článku
—