UV degradability of aryl-substituted polysilylenes
Popis výsledku v původním jazyce
The susceptibility of aryl-substituted polysilylenes to photodegradation by UV radiation at two different degradation wavelength ? = 355 and 266 nm is examined on poly[methyl(phenyl)silylene] (PMPSi), poly[(biphenyl-4-yl)methylsilylene] (PBMSi) and copolymer poly-[methyl(phenyl)silylene{3(4)-[(2,4-dinitrophenylhydrazono)methyl]phenyl}methylsilylene] (PMPSi-DNPH). The photodegradation of PMPSi by UV radiation decreases the intensity of the exciton photoluminescence (PL) band. The temporal dependence is in accord with the idea of the scission of longer Si-Si segments at points of #weak bonds#. Both degradation wavelengths cause the creation of unsaturated bonds of different origin both forming metastable states, susceptible to anneal. In PBMSi and PMPSi-DNPH, the visible photoluminescence first decreased during the degradation by UV radiation, similarly to that as in PMPSi caused by the absorption decrease, but then the rise and saturation of PL was observed. The model for the observed t
Název v anglickém jazyce
UV degradability of aryl-substituted polysilylenes
Popis výsledku anglicky
The susceptibility of aryl-substituted polysilylenes to photodegradation by UV radiation at two different degradation wavelength ? = 355 and 266 nm is examined on poly[methyl(phenyl)silylene] (PMPSi), poly[(biphenyl-4-yl)methylsilylene] (PBMSi) and copolymer poly-[methyl(phenyl)silylene{3(4)-[(2,4-dinitrophenylhydrazono)methyl]phenyl}methylsilylene] (PMPSi-DNPH). The photodegradation of PMPSi by UV radiation decreases the intensity of the exciton photoluminescence (PL) band. The temporal dependence is in accord with the idea of the scission of longer Si-Si segments at points of #weak bonds#. Both degradation wavelengths cause the creation of unsaturated bonds of different origin both forming metastable states, susceptible to anneal. In PBMSi and PMPSi-DNPH, the visible photoluminescence first decreased during the degradation by UV radiation, similarly to that as in PMPSi caused by the absorption decrease, but then the rise and saturation of PL was observed. The model for the observed t
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/1P05ME729" target="_blank" >1P05ME729: Studium syntéz a degradačních procesů v alkyl a aryl substituovaných polysilanech pro aplikace</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2005
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Natural and Arteficial Ageing of Polymers
ISBN
3-9808382-9-3
ISSN
—
e-ISSN
—
Počet stran výsledku
12
Strana od-do
297-308
Název nakladatele
Gesellschaft fuer Umweltsimulation e.V. GUS
Místo vydání
Karlsruhe
Místo konání akce
Gothenburg, Sweden
Datum konání akce
16. 6. 2005
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—